Lanthanum Strontium Aluminum Tantalum Oxide ( LSAT )
LSAT
LAST mat
LSA
Crystal properties
Crystal growth method
Czochralski
Crystal growth orientation
(100) (110) (111)
Orientation accuracy
± 0.5°
Crystal structure
cubic m3m Mixed Peroviskite
Approximately Molecular Form
(La0.3Sr0.7) (Al0.65Ta0.35)O3
Cell parameter
a = 7.737 Å
Melting point
2113° K
Density
6.64 g / cm3
Specific Heat
5.1 W / m·k
Thermal Expansion (10-6k-1)
8.2 (295° K) 11 (973° K)
Dielectric Constant (εr)
22.7 (291° K / 1 MHz) 21.7 (90° K / 10 kHz)
Dielectric loss (tgδ)
7.47 x 10-5 (90° K / 10 kHz)
Hardness (Mohs)
6.5
Color
None or Light yellow (if needed)