Zinc Telluride (ZnTe)
|
 |
Crystal properties
|
Crystal growth method
|
Seeded Vapor-Phase Free Growth Technology
|
Crystal growth orientation
|
(100) (110) (111) +/- 0.5°
|
Crystal structure
|
cubic, a = 6.1034Å
|
Growth direction
|
<111>
|
Specific resistivity
|
< 1 X 106 Ohm cm
|
Hall mobility
|
130 (h) cm2 / V / sec.
|
EPD
|
< 5 X 105 / cm2
|
Twin
|
Twin free
|
Orientation
|
Size
|
Polish
|
(100)
|
10*10*1mm3
|
Both sides
|
(110)
|
10*10*1mm3
|
Both sides
|
(111)
|
10*10*1mm3
|
Both sides
|
|
|